The University of Wolverhampton in the UK is equipping a new center of excellence for shaped-beam laser additive manufacturing at its Springfield campus. John Robinson, the university's commercialization manager for additive manufacturing research, disclosed the development ahead of Formnext 2026. The center is being built by the university in partnership with EOS and AMCM, with partial support from a regional innovation fund, and has now installed a 1.2 kW AMCM system equipped with an nLIGHT beam-shaping laser. During planning, the university considered adding binder jetting or cold spray processes but dropped the idea because of limited floor space, and ultimately chose to build on more than two decades of experience in laser powder bed fusion. The university entered laser powder bed fusion in 1999 with an EOS M250 and later added an M270 and a 400 W M290. Tungsten is the research entry point for the new system: the team melts single tracks on the powder bed with the laser, spreading energy over a larger area by changing the beam profile, and systematically varies laser power and scan speed while holding other conditions fixed, repeating the trials under each beam profile and using the machine's Gaussian beam setting as an internal reference. Robinson noted that one parameter combination produced an unexpectedly "good melt pool," but the team has not yet directly compared finished parts with those made on conventional systems, so the conclusions remain to be verified. The center's research approach does not treat beam shaping first as a means of raising productivity, but instead asks which materials become processable once the energy distribution within the spot changes, and what happens at the interface when two materials are joined. The single-track tungsten trials are a basic experiment within this line of thinking, and the 1.2 kW AMCM system with its nLIGHT beam-shaping laser forms the hardware foundation for the university's work in laser powder bed fusion.