Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →

AlMgSc (Scalmalloy) Aluminum Powder

Aluminum Alloy Powders · Metal Additive Manufacturing Powder

Scalmalloy is a scandium-modified aluminum-magnesium alloy developed by Airbus for aerospace AM, offering the highest strength of any printable aluminum: ~510 MPa UTS as-built with excellent ductility and corrosion resistance. Its Al-Mg-Sc-Zr chemistry creates nano-scale Al3Sc precipitates during printing, delivering a unique strength-density ratio without hot cracking. Scalmalloy is used for topology-optimized brackets, drone and satellite structures where every gram matters; published LPBF data show 510 MPa UTS, 495 MPa YS and 13% elongation. Scandium makes powder expensive — typically $200-400 per kg — and supply is concentrated. Buyers should verify scandium content (~0.66%) and request documentation on the powder producer's Sc supply chain.

Typical Applications

Aerospace lightweight structures High-performance racing parts

AlMgSc (Scalmalloy) Aluminum Powder - Key Properties

Chemical composition (wt%) Al bal · Mg 4-5 · Sc ~0.66 · Zr 0.3-0.5 · Mn 0.3-0.8
Density 2.67 g/cm³ (bulk)
Tensile strength (as-built) 510 MPa UTS · 495 MPa YS (median of 5 data points)
Elongation (as-built) 13% (median of 5 data points)
Hardness ~141 HV (as-built)
Particle size 20-63 µm
Production Gas atomization — scandium-controlled lots
Standards Airbus Scalmalloy® specification (proprietary alloy)
Family
Aluminum Alloy
Particle Size
20-63 µm
Process
Gas atomization

3 product offer(s) — 3 supplier(s)

Frequently Asked Questions

How much does Scalmalloy powder cost?

Scandium content drives the price: typically $200-400 per kg. Request current quotes from verified suppliers on this page — responses within 24 hours.

Is Scalmalloy stronger than AlSi10Mg?

Yes — as-built Scalmalloy (~510 MPa) substantially exceeds AlSi10Mg (~300 MPa) and even heat-treated AlSi7Mg, at comparable weight. It is the strongest printable aluminum alloy.

Does Scalmalloy need heat treatment?

No — Scalmalloy achieves its strength directly in the as-built condition via Al3Sc precipitation during printing, which simplifies post-processing.

What is Scalmalloy used for?

Weight-critical aerospace and motorsport structures, drones, satellite brackets and topology-optimized parts where the strength-to-weight ratio justifies the premium.

Why is Scalmalloy expensive?

Scandium is a rare, costly alloying element with concentrated supply. Prices reflect Sc market price; batch sizes are typically smaller than for standard aluminum alloys.

Need AlMgSc (Scalmalloy) Aluminum Powder?

Submit one request and verified suppliers quote you directly — usually within 24 hours. No obligation.

Request Quote — 24h Response

Market Reference

$62.00 – $213.50 / kg

Live EXW prices from 3 supplier(s), 2 quote(s).

Get Live Quotes