13-8Mo Stainless Steel Powder

Stainless Steel Powders · Metal Additive Manufacturing Powder

13-8Mo (PH 13-8 Mo, UNS S13800) is a precipitation-hardening martensitic stainless steel delivering high strength, toughness and corrosion resistance, widely specified for aerospace structural AM. Its low carbon and balanced Cr-Ni-Mo-Al chemistry allow H950-H1150 ageing to tune strength from 1,200 to 1,500 MPa with excellent notch toughness. LPBF as-built 13-8Mo prints with good crack resistance; solution annealing plus ageing develops the full mechanical envelope. Gas-atomized powder in 15-45 µm and 15-53 µm cuts is standard. Aerospace buyers should request chemistry per AMS 5864 and hydrogen content control for high-strength applications.

Typical Applications

Aerospace structural parts High-strength fasteners Tooling & molds Defense components

13-8Mo Stainless Steel Powder - Key Properties

Chemical composition (wt%) Fe bal · Cr 12.25-13.25 · Ni 7.5-8.5 · Mo 2-2.5 · Al 0.9-1.35 · C ≤0.05
Density 7.80 g/cm³ (bulk)
Tensile strength (aged) 1,200-1,500 MPa depending on ageing temperature
Hardness 40-47 HRC (aged)
Particle size 15-45 µm / 15-53 µm
Production Gas atomization (VIGA)
Standards AMS 5864 · UNS S13800 · EN 1.4534
Family
Stainless Steel
Particle Size
15-45 um / 15-53 um
Process
Gas atomization (GA / VIGA)

Frequently Asked Questions

How much does 13-8Mo powder cost?

13-8Mo AM powder typically quotes $60-120 per kg. Verified suppliers on this page provide current quotes, usually within 24 hours.

What heat treatment does printed 13-8Mo need?

Solution anneal (~927°C) followed by ageing: H950 for peak strength (~1,500 MPa), H1050/H1150 for balanced toughness. Always stress-relieve before support removal.

Why choose 13-8Mo over 17-4PH?

13-8Mo offers higher toughness at comparable strength and better transverse ductility — favored for fracture-critical aerospace components where 17-4PH toughness is insufficient.

Which particle size should I order?

15-45 µm for fine aerospace features; 15-53 µm general purpose. Specify your machine model in the inquiry.

What documentation do aerospace buyers need?

AMS 5864 chemistry certificate, particle-size distribution, oxygen/nitrogen/hydrogen analysis and full lot traceability.

Need 13-8Mo Stainless Steel Powder?

Submit one request and verified suppliers quote you directly — usually within 24 hours. No obligation.

Request Quote — 24h Response

Market Reference

Live quotes available on request. Submit an inquiry and suppliers will respond with current pricing.

Get Live Quotes