Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →

304L Stainless Steel Powder

Stainless Steel Powders · Metal Additive Manufacturing Powder

304L is the low-carbon version of 304 stainless steel (C ≤0.03% vs ≤0.08%). The reduced carbon suppresses chromium carbide precipitation during the thermal cycles of welding and printing, giving markedly better intergranular corrosion resistance — the most balanced "weldability + corrosion resistance" austenitic grade. In additive manufacturing the process window is mature: 304L covers general structural parts, chemical piping and MIM feedstock. Compared with 316L it sacrifices a little chloride pitting resistance but costs less, making it the economical default for non-marine general engineering. When buying, verify the actual carbon content (it must really meet the L grade), and for printing-grade powder check sphericity, oxygen content and inclusion cleanliness.

Free Research · Grade Profile
304L Stainless Steel Powder — process windows, market signals & buying checklist
Read the deep dive →

Typical Applications

General engineering Food processing Architectural parts

304L Stainless Steel Powder - Key Properties

Chemical composition (wt%) Fe bal · Cr 18-20 · Ni 8-12 · C ≤0.03 · Mn ≤2 · Si ≤1
Density ~7.93 g/cm³ (standard typical value)
Melting point ~1400-1450°C (standard typical value)
Particle size 15-53 µm (LPBF) · 53-150 µm (DED)
Production VIGA gas atomization / water atomization
Standards GB/T 20878 (022Cr19Ni10) · UNS S30403 · ASTM A240
Family
Stainless Steel
Particle Size
15-53 µm
Process
Gas atomization (GA / VIGA)

3 product offer(s) — 2 supplier(s)

Frequently Asked Questions

What is the difference between 304L and 316L powder?

316L adds 2-3% molybdenum, which raises chloride pitting and crevice corrosion resistance. 304L costs less and is sufficient for general structural parts, chemical piping, food and pharmaceutical equipment; choose 316L for marine or chloride-rich environments.

How do I confirm the powder really meets the L grade?

Ask the supplier for the mill certificate and check the measured carbon content (≤0.03%). For printed parts, verify density and inclusion levels on a test coupon before volume orders.

What particle size should I use for LPBF?

15-53 µm is the mainstream LPBF cut for 304L; DED typically uses 53-150 µm, and MIM uses finer feedstock powder. Confirm the cut matches your machine before ordering.

Need 304L Stainless Steel Powder?

Submit one request and verified suppliers quote you directly — usually within 24 hours. No obligation.

Request Quote — 24h Response

Market Reference

Live quotes available on request. Submit an inquiry and suppliers will respond with current pricing.

Get Live Quotes