The volume alloy304L is the world’s most-produced stainless — 18-8 chemistry (Cr 18-20, Ni 8-12) with carbon capped at 0.03%.
316L’s cheaper siblingSkip the 2-3% Mo of 316L when the environment is mild — 304L covers general engineering and food contact.
Easy to printWide LPBF process window at 15-53 µm; abundant supply keeps lead times short.

1 · Why 304L

304L is the general-purpose austenitic stainless: 18-20% Cr and 8-12% Ni give solid corrosion resistance at the lowest alloy cost in the stainless family. The "L" means carbon capped at 0.03%, avoiding sensitization during welding — and during printing.

For AM it is the economical choice wherever the environment is mild: general engineering, food processing and architectural parts. If your application involves chlorides or seawater, step up to 316L (Mo 2-3%) — otherwise 304L prints identically and costs less.

2 · Process & Particle Size

Gas-atomized 15-53 µm is the standard cut for LPBF. 304L prints on the same parameters as 316L with a wide, forgiving window — an ideal first material for shops moving into stainless AM.

Chlorides are the boundary. 304L pits in chloride environments; choose 316L for marine, chemical or coastal exposure.
Watch Mn and S. Austenitics vary in Mn/S for printability — confirm the powder’s Mn ≤ 2.0% and low S for clean melt pools.

3 · Applications & Market Signals

Platform demand runs through general engineering (brackets, housings, jigs), food processing (contact parts under FDA-compatible care) and architectural parts (decorative and structural).

MIM feedstock crossover. 304L powder demand spans AM and metal injection molding — suppliers serving both give buyers volume leverage.
Prototyping default. For functional prototypes of stainless parts, 304L is the low-cost first print before final-material qualification.

4 · Four-Point Buying Checklist

1 · Chemistry. Cr 18-20, Ni 8-12, C ≤ 0.03% per ASTM A240 / EN 1.4307.
2 · PSD. Full D10/D50/D90 — 15-53 µm for LPBF, 20-63 µm for EBM.
3 · Oxygen & flow. O ≤ 600 ppm typical; Hall flow under 20 s/50 g.
4 · Environment check. Confirm the service environment before committing to 304L — chlorides demand 316L.

FAQ · 304L

When should I choose 304L over 316L?

When the environment is mild — general engineering, indoor equipment, food contact without chlorides. 316L’s 2-3% Mo only pays off in chloride-containing or coastal environments.

Is printed 304L as strong as printed 316L?

Comparable — both print to roughly 600 MPa UTS as-built with excellent ductility; the real difference is corrosion resistance, not strength.

What particle size of 304L should I use?

15-53 µm for LPBF, 20-63 µm for EBM, 45-106 µm for DED. State your machine model in the RFQ.

Source 304L with confidence Post your requirement with full specification — verified suppliers respond within 24 hours. The more complete your spec, the faster the quotes.
Post a 304L Requirement → Suppliers →

Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.