AlSi7Mg Aluminum Alloy Powder
Aluminum Alloy Powders · Metal Additive Manufacturing Powder
AlSi7Mg (F357/A357) is a casting-grade aluminum alloy adapted for AM, offering higher ductility than AlSi10Mg with good weldability.
Typical Applications
Aerospace castings replacement
Automotive parts
Family
Aluminum Alloy
Particle Size
20-63 µm
Process
Gas atomization