PowderSight Research · Grade Profile EN HomeChinese Version
Grade Profile

AlSi7Mg (F357): The Aerospace Aluminum

The casting-equivalent alloy made printable — aerospace structural properties with the weight of aluminum.

Published 2026-11-26 · Data: PowderSight supplier catalog & industry sources · ~5 min read
Aerospace pedigreeThe AM sibling of A357 casting alloy — AMS 4289-grade chemistry specified for structural, weldable aluminum parts.
Balanced properties~352 MPa UTS as-built with ~9% elongation — strength and ductility tuned by heat treatment.
Weldable & repairableThe F357 family welds and laser-repairs well — a real advantage over 6xxx alloys.

1 · Why AlSi7Mg

AlSi7Mg (F357 / A357 family) is the aerospace-grade aluminum of additive manufacturing: the chemistry of the proven A357 casting alloy, re-engineered for powder. Si around 7% keeps the melt fluid and crack-resistant; Mg 0.4-0.7% buys heat-treatment response.

It is specified where aluminum AM parts must be structural and certified — castings replacement in aerospace and high-performance automotive. Compared with AlSi10Mg it trades a little strength for weldability, repair-ability and a long casting-service pedigree that regulators already know.

2 · Process & Particle Size

Standard supply is 20-63 µm gas-atomized powder (aerospace-controlled lots), with 15-45 µm for fine detail. The T6 route (solution + artificial ageing) tunes strength and ductility; HIP is common for castings-replacement parts.

Iron is the enemy. Fe above 0.15% forms brittle β-phase needles — insist on measured Fe per AMS 4289.
Drying discipline. Aluminum powder picks up moisture; store and feed dry to keep flowability.

3 · Applications & Market Signals

The demand split: aerospace castings replacement (brackets, housings, hydraulic manifolds) and automotive parts (chassis and powertrain brackets).

Castings-to-print migration. Programs are replacing machined A357 castings with printed F357 parts at lower buy-to-fly ratios.
Repair markets open. Weldability makes F357 a candidate for laser-clad repair of damaged castings — powder demand beyond new builds.

4 · Four-Point Buying Checklist

1 · Chemistry per AMS 4289 / EN AC-42200. Measured Si 6.5-7.5, Mg 0.4-0.7, Fe ≤ 0.15%.
2 · PSD. 20-63 µm standard, 15-45 µm for fine detail — match the machine.
3 · Moisture control. Confirm dry storage and inert-gas packing.
4 · Heat-treatment route. Agree T6 or HIP route with the supplier before volume.

FAQ · AlSi7Mg (F357)

What is the difference between AlSi7Mg and AlSi10Mg?

AlSi7Mg (F357) has lower silicon for better weldability and ductility, backed by the A357 casting pedigree — the aerospace structural choice. AlSi10Mg prints stronger as-built and dominates general-purpose aluminum AM.

What heat treatment does printed AlSi7Mg need?

T6 (solution treatment + artificial ageing) for tuned strength and ductility; HIP where porosity must be eliminated for castings-replacement parts.

What particle size of AlSi7Mg should I use?

20-63 µm is the standard aerospace cut; 15-45 µm for fine detail. Match the cut to your machine model.

Source AlSi7Mg with confidence Post your requirement with full specification — verified suppliers respond within 24 hours. The more complete your spec, the faster the quotes.
Post a AlSi7Mg Requirement → Suppliers →