Inconel 718 Nickel Superalloy Powder
Nickel & Superalloy Powders · Metal Additive Manufacturing Powder
Inconel 718 (UNS N07718, GH4169 in China) is the most widely used nickel superalloy in metal AM, specified for aerospace turbine hardware, oil-and-gas downhole tools and high-temperature structural parts up to 700°C. Its nickel-chromium base with niobium precipitation hardening delivers 950-1,000 MPa as-built tensile strength, and full AMS 5662 heat treatment lifts properties to wrought-equivalent levels. Published LPBF data show as-built Inconel 718 at 955 MPa UTS and 632 MPa YS with 29% elongation; heat treatment (solution + double ageing) raises strength to 1,200+ MPa. Gas-atomized powder in 15-45 µm and 15-53 µm cuts is standard. Gamma-prime precipitation makes Inconel 718 prone to cracking during printing on some machines — check that your supplier's powder has tight chemistry (Nb 4.75-5.5%) and low oxygen. For aerospace buyers, request powder per AMS 5662 / ASTM B637 with full traceability and per-lot particle-size distribution.
Typical Applications
Inconel 718 Nickel Superalloy Powder - Key Properties
| Chemical composition (wt%) | Ni 50-55 · Cr 17-21 · Fe bal · Nb+Ta 4.75-5.5 · Mo 2.8-3.3 · Ti 0.65-1.15 · Al 0.2-0.8 |
| Density | 8.19 g/cm³ (bulk) |
| Tensile strength (as-built) | 955 MPa UTS · 633 MPa YS (median of 10 data points) |
| Elongation (as-built) | 29.5% (median of 10 data points) |
| Hardness | ~290 HV (as-built) · 44 HRC after full HT |
| Particle size | 15-45 µm / 15-53 µm |
| Production | Gas atomization (VIGA) — low-oxygen lots |
| Standards | AMS 5662 · ASTM B637 · UNS N07718 |
10 product offer(s) — 6 supplier(s)
-
15-53μm · NULL (China)Quote$44.50–49.00per kg
-
Inconel 718 Nickel Superalloy Powder ✓ Verified15-53 μm · Peshing Advanced Metals (Jiangsu, China)Quote$128.00–149.50per kg
-
15-53μm · Shaanxi Guizidan New Material Co., Ltd. (Hanzhong, Shaanxi)QuotePrice on request
-
15-45μm · Xi'an Ouzhong Material Technology Co., Ltd. (Xi'an, Shaanxi)QuotePrice on request
-
Reference standard value · ZTT SRIM Additive Manufacturing Co.,Ltd. (Nantong, Jiangsu)QuotePrice on request
-
15-53μm · Xi'an Ouzhong Material Technology Co., Ltd. (Xi'an, Shaanxi)QuotePrice on request
-
Custom size · Xi'an Ouzhong Material Technology Co., Ltd. (Xi'an, Shaanxi)QuotePrice on request
-
53-106μm · Xi'an Ouzhong Material Technology Co., Ltd. (Xi'an, Shaanxi)QuotePrice on request
-
15-53,45-106,53-150μm · Zhongke Bulafei Material Technology (Dongguan) Co., Ltd. (Dongguan, Guangdong)QuotePrice on request
-
53-150μm · Shaanxi Guizidan New Material Co., Ltd. (Hanzhong, Shaanxi)QuotePrice on request
Frequently Asked Questions
What is the price of Inconel 718 powder?
Inconel 718 AM powder quotes depend on cut and certification level. Verified suppliers on this page quote you directly, usually within 24 hours.
What heat treatment does printed Inconel 718 need?
Standard AMS 5662 route: solution anneal at 980°C, then double ageing (720°C/8h furnace cool + 620°C/8h). This develops the gamma-double-prime strengthening needed for high-temperature service.
Can Inconel 718 replace cast/wrought 718?
With proper HIP and full heat treatment, LPBF Inconel 718 meets or exceeds wrought properties in most applications and is already flying in turbine and rocket components.
Which particle size is standard for Inconel 718?
15-45 µm for high-resolution LPBF; 15-53 µm as the general cut. For EBM, 45-106 µm. Tell suppliers your machine model to get the right recommendation.
Why does Inconel 718 crack during printing?
Solidification cracking in LPBF 718 usually traces to chemistry at the edge of spec or excessive residual stress. Tight Nb/C control, preheated builds and proper support design solve most cases — discuss with your powder supplier and machine OEM.
Need Inconel 718 Nickel Superalloy Powder?
Submit one request and verified suppliers quote you directly — usually within 24 hours. No obligation.
Request Quote — 24h ResponseMarket Reference
Live EXW prices from 6 supplier(s), 2 quote(s).
Get Live Quotes