Holdson, based in West Yorkshire, UK, is selling electrochemical polishing equipment under the Electroform brand and also offers small-batch polishing services. Founded in 2023, the company began with a turbocharger project in collaboration with engine manufacturer Cummins, aimed at improving the surface finish of internal turbocharger surfaces. Holdson says metal additive manufacturing accounts for about 60% of its business, with aerospace making up the largest share; inquiries come mainly from engine manufacturers and their tier-one suppliers, and the most commonly involved materials are Inconel and titanium alloys. In terms of process, Holdson encloses a conventional polishing bath in a standalone unit. The electrolyte is primarily water-based salts with a small amount of additives, and the specific formulation depends on the material being processed. The workpiece serves as the anode, current flows through the electrolyte between the workpiece and a second electrode, and metal preferentially dissolves at the high points of rough surfaces. For a typical additive manufacturing part with an average surface roughness (Ra) of 10–15 µm, Holdson can reduce it to below 5 µm in about 20 minutes; longer cycles can bring some surfaces to about 1 µm Ra. Material removal depends on the starting surface condition and ranges from a few microns to about 300 µm. For internal channels as small as about 2 mm in diameter, whether the electrode can reach inside and whether the electrolyte can flow through the channel are just as critical as the dimensions on the drawing. Metal additive manufacturing allows engineers to print internal geometries that are difficult to access after forming, which is exactly where Holdson's electrochemical polishing process comes in. The company handles cast, formed and machined parts, and the demand for polishing internal channels created by additive manufacturing corresponds directly to the capabilities it built up in the Cummins turbocharger project.