Preparation and Industrialization of 3D-Printed Tungsten Alloy Powder for the Nuclear Industry
📰 News Source
This article was translated from a Chinese source.
Source URL not available
Show Chinese original
核工业专用3D打印钨合金粉末制备与产业化项目
核工业专用3D打印钨合金粉末制备与产业化项目(项目代码 2608-330424-04-01-402928)在企业投资项目备案平台公示,建设地点为浙江省嘉兴市海盐县。项目为核工业专用的钨合金(难熔金属)粉末制备与产业化,属产能扩张。