America Makes, in partnership with NCDMM, has announced the winners of the 2026 Organic Industrial Base (OIB) Modernization Challenge, with total awards reaching $15 million. Funded by the U.S. Department of Defense's Manufacturing Technology (OSD ManTech) program, the challenge prioritizes advanced technologies including additive manufacturing, digital operations, AI-driven planning, and in-situ quality inspection, with the goal of accelerating the transition of mature technologies into the OIB. The initiative aims to strengthen the defense industrial base, boost production efficiency, and enhance supply chain resilience—delivering a direct impact on defense applications within the metal additive manufacturing sector.