Yunlu Co., Ltd. (688190) was granted a utility model patent on July 24, 2026, for equipment titled 'A Continuous Casting Gas Atomization Powder Production Device,' with patent application number CN202521701726.8. The device comprises core components such as an atomization tower, first and second medium-frequency furnaces, a tundish, powder delivery piping, a cyclone separator, a small material tank, a cooling unit, a mobile material tank, a dust collector, and a fan. Its core technical principle is that while the first medium-frequency furnace is casting, the second furnace concurrently charges and melts steel; once the first furnace completes casting, the second is ready to pour, enabling a cyclic multi-furnace continuous casting process. This patent addresses the technical challenge of continuous casting in conventional gas atomization powder production equipment, ensuring production efficiency. Yunlu Co., Ltd., a national-level specialized and new 'Little Giant' enterprise under AECC, primarily produces advanced magnetic metal materials such as amorphous alloy ribbons, nanocrystalline alloys, and atomized powders. This year, the company has received 15 new patent grants, a 275% increase year-over-year, with R&D investment of 119 million RMB in 2025. This patent represents a core technological breakthrough in gas atomization powder production equipment, further enhancing the efficiency and continuity of powder production.