Austrian company Incus expands metal additive manufacturing capabilities through Lithography-based Metal Manufacturing (LMM) technology. This technology uses photosensitive metal powder slurry for layer-by-layer curing and forming, enabling the production of high-precision complex metal parts. Compared to traditional powder bed fusion processes, LMM achieves finer details and smoother surface quality, suitable for precision applications such as medical and jewelry sectors.