Hefei Innowinano has filed a patent for multi-material micro 3D printing to produce lightweight, conformal automotive wiring harnesses that fully adhere to vehicle structures, offering reduced bending stress and improved durability. The patent (CN121983390A), filed in February 2026, involves direct printing of wiring harnesses on curved substrates, enhancing assembly automation, lowering labor costs, and facilitating mass production. For the metal powder industry, this multi-material printing trend will drive the development of customized powders. In downstream automotive manufacturing, it simplifies wiring processes for tight spaces, with future applications expected in new energy vehicles and smart cabins. Founded in 2025, the company's technology originates from Professor Lan Hongbo's team at Qingdao University of Technology, utilizing electric-field-driven jet deposition for micro-nano 3D printing.