The national standard GB/T 47570-2026 "Metal Additive Manufacturing — Qualification Principles — Qualification of Coordinators" will come into effect on August 1, 2026. This standard is under the jurisdiction of the National Additive Manufacturing Standardization Technical Committee (TC562) and is identical to the international standard ISO/ASTM 52935:2023. The main drafting organizations include China Machine Productivity Promotion Center Co., Ltd., Xi'an Bright Laser Technologies Co., Ltd., and others. The standard specifies the qualification requirements for coordinators in metal additive manufacturing qualification principles, providing a unified regulatory basis for the industry's quality system. It aligns China's metal additive manufacturing with international practices in personnel qualification and quality control, helping to enhance the recognition of domestic metal 3D-printed products in the global supply chain.