At Formnext 2026 (Hall 11.0, Booth A55), Continuum Powders unveiled Argos, its next-generation melt-based powder production platform. Argos combines cold-crucible plasma melting with inert gas atomization, featuring a melting power of over 0.5 MW and a designed daily output of more than 4 tons of metal powder, targeting the large-scale continuous production demands of additive manufacturing. The platform is equipped with the Max DP atomization die, a satellite-particle suppression system optimized through computational fluid dynamics, and automatic pouring technology. The first validated material is OptiPowder 718 nickel-based superalloy, which has already been certified for the HP Metal Jet S100. Argos will run in parallel with the existing Greyhound platform. CEO Jon Cozens says the system is aimed at securing qualified powder supply for high-demand alloys. Continuum uses recycled feedstock and green electricity, positioning itself around low-carbon, large-scale powder production. Grades such as Ni718 and titanium alloys, which involve long qualification cycles and high supply risk, will gain a second supply source, helping powder buyers diversify supply risk and strengthen their negotiating position.