At Formnext 2026 (Hall 12.1, Booth D41), HP announced an expansion of its Metal Jet binder jetting material system: OptiPowder Ni718 nickel-based superalloy has passed certification for the HP Metal Jet S100, OptiPowder M247LC has entered the certification process, and HP is collaborating with GKN Powder Metallurgy to advance copper alloy printing (3DPrint.com, November 17 report). Ni718 was jointly certified by Continuum Powders and INDO-MIM, with printed parts achieving density above 98% and hardness of 74-79 HR15N; the copper printing effort targets data center thermal management applications, leveraging binder jetting's cost advantages for volume production of high-thermal-conductivity copper components. At the same event, HP also launched the IF 600HT industrial fused deposition modeling system, expanding its portfolio across multiple technology routes in parallel. The binder jetting route places different demands on powder sintering characteristics and batch consistency than conventional LPBF, meaning certification thresholds effectively become supply thresholds. The expansion of the certified BJ printing material list for Ni718 and copper opens new volume production supply channels for powder manufacturers that have already obtained or are applying for HP certification, while uncertified powder producers should begin benchmark testing as early as possible.