Eplus3D has partnered with Oqton to improve the compatibility between 3DXpert software and Eplus3D laser powder bed fusion systems. The two sides are focusing on applying MeltControl technology and enabling a direct connection from software to equipment. 3DXpert's MeltControl uses physics-driven local scan path optimization, adaptively adjusting energy input based on downward-facing angles and local thermal conditions to reduce reliance on conventional support structures. The two companies successfully printed a complex fuel tank in IN718 alloy on the EP-M300 system, validating the feasibility of this strategy on Eplus3D hardware.