Horkos and Spanish metal 3D printing company Meltio have jointly launched the NX70 Duo version AM dual-head bedless hybrid machining center, which integrates wire-laser metal deposition additive manufacturing with high-precision cutting in a single machine. The first unit has completed a commercial sale to a major industrial customer with operations in international markets. The system is based on Horkos's NX70 1510B machining center and uses Meltio's wire-based directed energy deposition (Wire-DED) technology, in which welding wire serves as the raw material and laser energy is used to precisely deposit material where needed. It supports a two-stage manufacturing process in which additive and subtractive operations alternate within the same setup. The machine combines Horkos's proprietary bedless compact structure with a water-soluble iMQL system, making it suitable for the production, repair, remanufacturing, and prototyping of complex parts with limited tool access, such as closed impellers. Potential applications span aerospace, defense, energy, and heavy industry. The integration builds on the continued expansion of Meltio's DED technology in CNC manufacturing environments: Phillips Federal in the United States has, in a single transaction, sold 12 hybrid manufacturing systems based on the Haas TM-1P CNC platform with integrated Meltio metal DED technology to the U.S. Navy training base in Danville, Virginia, for training Navy personnel in metal hybrid manufacturing to support fleet maintenance, repair, and on-demand production. The integration of the NX70 Duo version AM was supported by MadeHere, Meltio's official partner in Japan.