Rostec, Russia's state technology group, announced on November 12 that its subsidiary United Engine Corporation (ODK) has transitioned to unified standards for metal 3D printing equipment used in the production of aircraft engine parts. The standards were developed by ODK's Additive Technology Center (CAT) together with the group's various plants and institutes, establishing evaluation criteria for the organization, design and software solutions of selective laser melting (SLM) equipment, the modularization of optical systems, and the consistency of process parameters. The goal is to unify manufacturing process preparation and make printing modes portable across equipment from different manufacturers, thereby simplifying the mass production certification process (moving from per-part, per-machine certification to overall certification of the production system), improving product quality, and expanding the use of 3D printing in engine manufacturing. Before equipment is admitted to the unified technology platform, it must undergo evaluation and testing covering documentation completeness, quality management systems, measured performance, and sample parts. The platform concept was first presented at INNOPROM India in September 2026, has already attracted more than five Russian equipment manufacturers, and is being jointly validated for material performance with the All-Russian Institute of Aviation Materials (VIAM).