Snowbird Technologies has released the cost and lead time results of its metal 3D printing participation in the RIMPAC 2026 exercise. The US deployable manufacturing systems manufacturer produced metal replacement parts using its SAMM Tech hybrid manufacturing platform aboard the amphibious assault ship USS Essex and at Schofield Barracks Army base in Hawaii. The exercise was organized by the US Naval Postgraduate School (NPS) Consortium for Advanced Manufacturing Research and Education (CAMRE) and the FLEETWERX program to evaluate the feasibility of expeditionary additive manufacturing producing parts close to the point of need. The company reported that four of seven parts were manufactured at a lower cost than purchasing them. The SAMM Tech platform integrates the Meltio Engine Blue wire-laser metal additive manufacturing system developed by Spanish metal 3D printing company Meltio, which deposits material using metal wire feedstock and a laser energy source, with nitrogen used as the process gas during the exercise. The platform produced seven unique parts, including oxygen cylinder brackets, drain caps, load test fixture assemblies, turnbuckles, four-inch pipe flanges, and a six-unit rack for airfield radios. Producing 12 oxygen cylinder brackets took about 75 hours and consumed approximately USD 2,492 in wire and gas costs, compared with a purchase cost of USD 9,624 from Pearl Harbor Naval Shipyard (PHNSY) and USD 10,224 for supply to USS Essex. The outer load test fixture assembly took about 3 hours to manufacture at a cost of USD 101, versus purchase costs of USD 420 and USD 455 respectively; the inner load test fixture assembly took about 9 hours to print at a cost of USD 289, with the same purchase costs. The six-unit airfield radio rack took 5 hours to manufacture at a cost of USD 154, versus purchase costs of USD 624 and USD 654. The company reported savings of up to 351%, a figure that represents the cost premium of purchasing relative to additive manufacturing rather than a conventional percentage cost reduction. In the case of two turnbuckle external assemblies, local production took about 28 hours at a wire and gas cost of USD 902, higher than the estimated USD 590 cost of purchasing from USS Essex. Nevertheless, the company reported avoiding 692 hours of procurement waiting time. The exercise results directly relate to the wire-laser directed energy deposition (DED) process as an alternative to metal powder in military expeditionary scenarios, using metal wire rather than metal powder as feedstock and validating the cost structure and lead times for on-demand manufacturing of metal parts under shipboard and shore-based conditions.