New Strategy for IN718 Laser Directed Energy Deposition: Layer-Synchronized Induction Heating Achieves Continuous Homogenization
📰 News Source
This article was translated from a Chinese source.
Source URL not available
Show Chinese original
IN718激光定向能量沉积新策略:层同步感应加热实现连续均匀化
《Additive Manufacturing》刊发新策略:在激光定向能量沉积(LDED)过程中及之后施加层同步感应加热,对IN718实现连续均匀化,抑制Nb/Mo/Ti偏析导致的Laves相有害析出,为替代沉积后炉内均匀化热处理、提升蠕变性能提供新路径。