Aluminum Powder for Additive Manufacturing

Your complete guide to aluminum alloy powders: AlSi10Mg, Al7075, Scalmalloy, and A20X. Compare mechanical properties, PSD requirements, pricing based on PS Price Index data, heat treatment protocols, and find verified Chinese manufacturers with competitive EXW pricing.

¥65–550
EXW Price (CNY/kg)
20–63µm
Typical LPBF PSD
VIGA
Production Method
Auto/Heat Exch.
Key Applications

1. Aluminum Powder Grades Compared

Aluminum alloys are the most cost-effective entry point into metal additive manufacturing. They offer excellent thermal conductivity, low density, and good mechanical properties at a fraction of titanium's cost. The challenge is managing the high reflectivity and thermal conductivity during printing.

GradeUTS (MPa)ElongationPrice (CNY/kg)Best For
AlSi10Mg320–4603–8%¥65–100Automotive, heat exchangers, general prototyping
Al7075480–5705–11%¥90–150High-strength structural, aerospace secondary
Scalmalloy480–5408–13%¥350–550Aerospace, high-fatigue, racing
A20X410–4704–7%¥180–300High-temperature (up to 250°C), aerospace
💡 PS Price Index Data (2026): AlSi10Mg is the workhorse of aluminum AM — accounting for ~70% of all aluminum powder orders. The PS Price Index shows a median of ¥80/kg for AlSi10Mg 15–53µm VIGA (9 verified quotes, latest: 2026-04-20). Chinese suppliers offer it at ¥65–100/kg, which is significantly lower than Western sources while meeting the same chemistry specs. Scalmalloy remains premium-priced due to APWorks' IP and limited production capacity.

2. Heat Treatment — Critical for Aluminum AM Parts

Unlike titanium where as-built properties are often sufficient, aluminum AM parts almost always require post-process heat treatment to relieve residual stress and optimize mechanical properties.

T6 (Solution + Aging): Standard for AlSi10Mg. Solution treat at 520–540°C for 1–2 hours, water quench, then age at 155–175°C for 6–12 hours. Achieves maximum strength but may cause distortion in thin-walled parts.
Stress Relief (SR): 280–300°C for 2 hours. Lower strength than T6 but minimal distortion. Preferred for complex geometries with thin walls.
Hot Isostatic Pressing (HIP): 450–500°C at 100 MPa. Eliminates internal porosity for fatigue-critical parts. Adds ¥30–60/kg to final cost.

3. Key Applications by Industry

🚗 Automotive

Lightweight brackets, heat exchangers, suspension components. AlSi10Mg dominates. Serially produced by BMW, Mercedes, Porsche.

🚀 Aerospace

Secondary structures, UAV components, antenna brackets. Scalmalloy or A20X for high-strength; AlSi10Mg for non-critical.

🔥 Thermal Management

Conformal cooling channels, heat sinks, cold plates. AlSi10Mg's thermal conductivity (140–170 W/mK) is ideal.

🏭 Industrial Tooling

Conformal cooling inserts for injection molds. AlSi10Mg provides 30–40% cycle time reduction vs. conventional cooling.

Get Competitive Quotes for Aluminum Powder

Specify your grade, PSD, and volume. We'll match you with pre-vetted Chinese manufacturers in 24 hours.

Request Aluminum Powder Quotes →