Al-Mg-Sc Alloy Powder

Aluminum Alloy · Al-Mg-Sc · 15-53μm

Price Range / 价格区间

$0.00 - $0.00 / 元/公斤

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
Al-Mg-Sc
Particle Size
15-53μm
Process
真空气雾化法

Technical Specifications / 技术规格

Grade: Al-Mg-Sc | Particle Size: 15-53μm | Process: 真空气雾化法 | Application: 航空航天、汽车制造、3D打印轻量化结构件、支架类、阀体等

Compare Similar Products

Product Particle Size Price (USD/kg) Supplier Certifications
Al-Mg-Sc Alloy Powder Current 15-53μm $0 – $0 Advanced Technology & Materials (AT&M) —
AlSi(5-70) Aluminum-Silicon Alloy Powder for Additive Manufacturing 20-63um $10 – $22 Hunan AoKe New Material Technology Co., Ltd. ✓ — Compare →
AlSi10Mg Aluminum Alloy Powder for Additive Manufacturing 20-63μm $12 – $12 Inner Mongolia Sunruns New Material Co., Ltd. ✓ — Compare →
6061 Aluminum Alloy Powder for Additive Manufacturing 20-63um $12 – $15 Hunan AoKe New Material Technology Co., Ltd. ✓ — Compare →
2024 Aluminum Alloy Powder for Additive Manufacturing 20-63um $20 – $34 Hunan AoKe New Material Technology Co., Ltd. ✓ — Compare →
7075 Aluminum Alloy Powder for Additive Manufacturing 15-53um $26 – $38 Hunan AoKe New Material Technology Co., Ltd. ✓ — Compare →

📊 Price Trend — Aluminum Alloy

Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.

🔗 Related Aluminum Alloy Products