Titomic's U.S. subsidiary has received an order from EOS Defense Systems USA to supply critical components for its U.S. defense production program, with delivery completed within one week. The order value was not disclosed. The order involves the rapid re-manufacturing of critical components using cold spray additive manufacturing. Cold spray is a solid-state deposition process used to fabricate and repair metal parts without melting the material. Rapid re-manufacturing and short-lead-time delivery of defense spare parts are typical applications of cold spray technology. This order validates the practical value of cold spray in the defense supply chain. Value for powder buyers: ① Demand for metal powders used in cold spray (aluminum, copper, titanium and their alloys) is linked to the defense repair market—relevant grades and particle sizes should be monitored. ② Domestic cold spray equipment and powder suppliers may find opportunities in the military repair sector. ③ As the order value was not disclosed, ongoing monitoring is needed to determine whether sustained orders will follow, which would clarify the scale of powder demand.