Sichuan Shangcai 3D New Material Technology Co., Ltd. has achieved a major breakthrough in gas atomization powder production technology, with the yield of spherical titanium powder below 60 microns exceeding 90% and achieving stable production. Previously, the industry-standard yield was only 60-70%. In 2018, imported spherical titanium powder was priced as high as 3,000 RMB/kg. Following this breakthrough, the price has dropped to around 200 RMB/kg, reducing overall usage costs by 30% on raw materials alone, transforming high-end titanium powder from an 'expensive niche material' into a fundamental raw material suitable for large-scale applications, breaking the foreign monopoly. Leveraging its independently developed electrode induction melting gas atomization system, high-pressure high-purity argon recovery system, and metal powder high-cleanliness surface treatment and classification system, the company's products are now used in bulk across aerospace, semiconductors, medical devices, consumer electronics, and other fields.