Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →
✈️

Ti-6Al-4V ELI Grade 23 Medical Powder

✓ Verified

Titanium Alloy · Ti-6Al-4V ELI (Grade 23) · 15-53 μm

Price Range / 价格区间

$159.00 - $191.50 / per kg

MOQ: 5 kg

Lead Time: 10-14 days

● In Stock

Grade
Ti-6Al-4V ELI (Grade 23)
Particle Size
15-53 μm
Process
EIGA

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified
ISO 9001 AS9100D ISO 13485

Technical Specifications / 技术规格

Chemical: Ti Bal, Al 5.50-6.50%, V 3.50-4.50%, O <=0.13% (ELI) | PSD: 15-53 μm | UTS: >=860 MPa | YS: >=795 MPa | Elongation: >=10% | Biocomp: ISO 10993, ASTM F136

Description / 产品描述

Ultra-low interstitial (ELI) Ti-6Al-4V Grade 23 powder for medical implant applications. Reduced oxygen content for improved ductility and fracture toughness.

Compare Similar Products

Product Particle Size Price (USD/kg) Supplier Certifications
Ti-6Al-4V ELI Grade 23 Medical Powder Current 15-53 μm $159 – $192 Avimetal Powder Technology ✓ ISO 9001AS9100DISO 13485
TC11 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $52 NULL ✓ — Compare →
TA15 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $49 NULL ✓ — Compare →
Ti-6Al-4V Spherical Powder for Aerospace AM 15-53 μm $90 – $102 Avimetal Powder Technology ✓ ISO 9001AS9100D Compare →

📊 Price Trend — Titanium Alloy

Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.

🔗 Related Titanium Alloy Products