Ti-6Al-4V Spherical Powder for Aerospace AM
Titanium Alloy · Ti-6Al-4V (Grade 5) · 15-53 μm
Price Range
MOQ: 10 kg
Lead Time: 7-10 days
● In Stock
Technical Specifications
Description
Ti-6Al-4V (Grade 5 / TC4) spherical titanium alloy powder for aerospace, medical and high-performance engineering. The workhorse AM alloy: ~950 MPa UTS at 4.43 g/cm3 — the best strength-to-weight ratio among common AM metals. Gas-atomized 15-53 um and 15-45 um cuts with high sphericity, low oxygen (<1300 ppm) and tight PSD for L-PBF, EBM and DED. Used in airframe brackets, turbine components, implants (ELI grade) and motorsport parts. Chemistry per ASTM F2924; ELI variants per ASTM F3001 for medical. Request batch PSD, oxygen and flowability reports.
Compare Similar Products
| Product | Particle Size | Price (USD/kg) | Supplier | Certifications | |
|---|---|---|---|---|---|
| Ti-6Al-4V Spherical Powder for Aerospace AM Current | 15-53 μm | $90 – $102 | Avimetal Powder Technology ✓ | ISO 9001AS9100D | |
| TC11 Titanium Alloy Powder for Additive Manufacturing | 75-250μm | $44 – $52 | NULL ✓ | — | Compare → |
| TA15 Titanium Alloy Powder for Additive Manufacturing | 75-250μm | $44 – $49 | NULL ✓ | — | Compare → |
| Ti-6Al-4V ELI Grade 23 Medical Powder | 15-53 μm | $159 – $192 | Avimetal Powder Technology ✓ | ISO 9001AS9100DISO 13485 | Compare → |