Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →
✈️

Ti-6Al-4V Spherical Powder for Aerospace AM

✓ Verified

Titanium Alloy · Ti-6Al-4V (Grade 5) · 15-53 μm

Price Range / 价格区间

$90.00 - $101.50 / per kg

MOQ: 10 kg

Lead Time: 7-10 days

● In Stock

Grade
Ti-6Al-4V (Grade 5)
Particle Size
15-53 μm
Process
EIGA

Supplier / 供应商

A

Avimetal Powder Technology

Jiangsu, China

Verified
ISO 9001 AS9100D

Technical Specifications / 技术规格

Chemical: Ti Bal, Al 5.50-6.75%, V 3.50-4.50%, Fe <=0.30%, O <=0.13%, N <=0.05% | PSD: D10 >=10μm, D50 30-35μm, D90 <=55μm | App Density: >=2.7 g/cm³ | Flow: <=35 s/50g | Sphericity: >=0.92 | UTS: 900-1100 MPa

Description / 产品描述

Premium grade Ti-6Al-4V (Grade 5) spherical powder optimized for SLM and EBM. Produced via EIGA process ensuring ultra-low oxygen content and excellent flowability. Ideal for aerospace structural components, medical implants, and high-performance automotive parts.

Compare Similar Products

Product Particle Size Price (USD/kg) Supplier Certifications
Ti-6Al-4V Spherical Powder for Aerospace AM Current 15-53 μm $90 – $102 Avimetal Powder Technology ✓ ISO 9001AS9100D
TC11 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $52 NULL ✓ — Compare →
TA15 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $49 NULL ✓ — Compare →
Ti-6Al-4V ELI Grade 23 Medical Powder 15-53 μm $159 – $192 Avimetal Powder Technology ✓ ISO 9001AS9100DISO 13485 Compare →

📊 Price Trend — Titanium Alloy

Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.