Titanium Powder for Additive Manufacturing

Everything you need to know about sourcing titanium alloy powders: Ti-6Al-4V, Grade 23 ELI, Ti5553, CP-Ti. Compare grades, PSD specs, production methods, pricing based on PS Price Index data, and find verified Chinese manufacturers.

¥180–500
EXW Price (CNY/kg)
15–53µm
Typical LPBF PSD
VIGA/EIGA
Production Method
ASTM F2924
Key Standard

1. Titanium Powder Grades — Which One Do You Need?

Titanium alloys dominate aerospace and medical additive manufacturing due to their exceptional strength-to-weight ratio, biocompatibility, and corrosion resistance. Selecting the right grade depends on your application requirements for tensile strength, elongation, and fatigue life.

GradeCompositionUTS (MPa)Price (CNY/kg)Typical Applications
TC4 / Ti-6Al-4V Grade 5Ti + 6% Al + 4% V950–1050¥180–280Aerospace structural, turbine blades, automotive
Ti-6Al-4V Grade 23 ELITi + 6% Al + 4% V (extra-low interstitial)860–965¥220–350Medical implants, spinal cages, trauma plates
Ti5553 (Ti-5Al-5V-5Mo-3Cr)Ti + 5Al + 5V + 5Mo + 3Cr1100–1250¥280–450Landing gear, high-strength airframe
CP-Ti Grade 2 / TA2Commercially pure Ti345–450¥350–500Chemical processing, heat exchangers
💡 PS Price Index Data (2026): TC4 15–53µm median price is ¥200–205/kg across 18 verified quotes (latest: 2026-07-10). TA2 median is ¥400/kg. Grade 23 ELI is the medical-grade variant of Ti64 — the "extra-low interstitial" specification limits oxygen and iron content, improving ductility and fracture toughness. Expect a 15–25% price premium over standard Grade 5.

2. PSD Specifications & Production Methods

Particle Size Distribution (PSD)

The PSD you need depends entirely on your printer technology. Titanium is reactive in fine powder form, so finer PSDs carry a safety premium.

TechnologyRecommended PSDLayer Thickness
LPBF / SLM15–45µm or 15–53µm30–60µm
EBM (Electron Beam Melting)45–105µm50–100µm
DED (Directed Energy Deposition)53–150µm250–1000µm
Binder Jetting<45µm (fine cut)50–100µm

Production Methods

VIGA (Vacuum Induction Gas Atomization)

Most common. Good sphericity, moderate cost. Suitable for non-critical aerospace and industrial applications. Some oxygen pickup risk with reactive metals.

EIGA (Electrode Induction Gas Atomization)

Preferred for titanium. No crucible contact → minimal contamination. Higher purity, better sphericity. Premium price but required for aerospace and medical.

PREP (Plasma Rotating Electrode Process)

Highest sphericity and flowability. Very low oxygen content. Narrow PSD. Most expensive — reserved for fatigue-critical rotating parts.

PA (Plasma Atomization)

Excellent sphericity using Ti wire feedstock. Low satellite particles. Good for demanding aerospace specs. Mid-to-high price range.

3. Certifications & Quality Standards

Titanium powder for critical applications must meet rigorous certification requirements. Always request certificates before placing an order.

  • ✓ASTM F2924 — Standard specification for Ti-6Al-4V powder for additive manufacturing. Covers chemistry, PSD, and impurity limits.
  • ✓ASTM F3001 — Standard specification for Ti-6Al-4V ELI (Grade 23) powder. Required for medical implant applications.
  • ✓ISO 5832-3 — Implants for surgery — Ti-6Al-4V alloy. International medical device standard.
  • ✓AMS 4998 — Aerospace Material Specification for Ti-6Al-4V powder. Required by major aerospace OEMs.
  • ✓ISO 13485 — Medical device quality management system. Essential for medical-grade powder suppliers.

4. Titanium Powder Pricing — What Affects Cost?

Titanium powder pricing is influenced by multiple factors. Understanding these helps you negotiate better and avoid overpaying. All prices below are based on PS Price Index data from verified Chinese manufacturer quotes.

Production Method

EIGA and PREP cost 30–60% more than VIGA due to lower throughput and higher purity. Plasma atomization adds another 20–40%. PS Index: VIGA TC4 median ¥200–205/kg; PREP TC4 median ¥205/kg.

PSD Range

Finer cuts (15–45µm) cost 15–25% more than standard (15–53µm). Each additional classification step adds cost.

Order Volume

MOQ typically 5–10 kg. Pricing drops 10–15% at 100 kg, 20–30% at 500 kg. Spot buys pay a premium.

Certification Level

Full certs (chemistry + PSD + flow + morphology) add ¥30–60/kg. AMS/medical certs add ¥60–120/kg.

📊 PS Price Index Data (2026): TC4 titanium powder 15–53µm median is ¥200–205/kg (18 verified quotes). Chinese titanium powder prices are typically 20–40% below Western suppliers for equivalent quality. EIGA-produced Ti64 from verified Chinese manufacturers now meets ASTM F2924 and is approved by multiple aerospace OEMs.

Need Titanium Powder? Compare Quotes from Verified Suppliers

Tell us your grade, PSD, and volume — we match you with qualified Chinese manufacturers in 24 hours.

Get Titanium Powder Quotes →

Grade pages — specs, live prices & suppliers