Titanium Alloy Powder

Titanium Alloy · TC4 MIM Powder · 0-25μm

Price Range

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
TC4 MIM Powder
Particle Size
0-25μm
Process
PA Plasma Atomization

Technical Specifications

Grade: TC4-MIM powder | Particle Size: 0-25μm | Process: PA plasma atomization | Application: MIM parts

Compare Similar Products

Product Particle Size Price (USD/kg) Supplier Certifications
Titanium Alloy Powder Current 0-25μm $0 – $0 Avimetal Powder Technology —
TC11 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $52 NULL ✓ — Compare →
TA15 Titanium Alloy Powder for Additive Manufacturing 75-250μm $44 – $49 NULL ✓ — Compare →
Ti-6Al-4V Spherical Powder for Aerospace AM 15-53 μm $90 – $102 Avimetal Powder Technology ✓ ISO 9001AS9100D Compare →
Ti-6Al-4V ELI Grade 23 Medical Powder 15-53 μm $159 – $192 Avimetal Powder Technology ✓ ISO 9001AS9100DISO 13485 Compare →

📊 Price Trend — Titanium Alloy

Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.

🔗 Related Titanium Alloy Products