SUPERFLOW® CP-Ti

Titanium Alloy · TA1 · 20-63μm

Price Range / 价格区间

$0.00 - $0.00 / 元/公斤

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
TA1
Particle Size
20-63μm
Process
使用增材制造技术(SLM/EBM)进行加工,直接成型

Technical Specifications / 技术规格

Grade: TA1 | Particle Size: 20-63μm | Process: 使用增材制造技术(SLM/EBM)进行加工,直接成型 | Application: 医疗用人体植入物和轻质量的中小型零件、医疗器械、齿科等