HF20263473 Award Announcement for Additive Manufacturing of GH4099 Lightweight Rudder-Wing Structures
On November 20, 2026, the School of Mechanical Science and Engineering at Huazhong University of Science and Technology issued an award announcement for the additive manufacturing of GH4099 lightweight rudder-wing structures. The winning supplier is Shaanxi Yandiao Additive Manufacturing Co., Ltd., with a contract value of 67,000 RMB. The project requires additive manufacturing of key sections of a honeycomb-skeleton-filled rudder surface structure and a hollow lattice-filled wing surface structure. Payment terms are 100% of the contract amount within 10 working days after the service is completed and accepted. The formed parts are made of a superalloy using the metal selective laser melting process. The outer contour of the honeycomb-skeleton-filled rudder surface structure model must be no smaller than 380 mm long by 346 mm wide by 67 mm high, and the outer contour of the hollow lattice-filled wing surface structure model must be no smaller than 299 mm long by 30 mm wide by 257 mm high. Both formed parts require a surface roughness of Ra 6.3 micrometers or better, with no cracks, porosity, or burrs on the surface. The service period is 25 working days from contract signing. The announcement specifies GH4099 superalloy as the forming material and metal selective laser melting as the manufacturing process for the lightweight rudder-wing structures. The supplier must complete the additive manufacturing of the two key parts within 25 working days and meet the specified surface quality indicators.