Velori Launches Diamond-Copper Powder, Completing Four Copper-Based Product Categories for AI Computing Thermal Management
Jiangsu Velori New Materials officially launched diamond-copper powder at the AMTAE exhibition in Luzhou, completing its copper-based product line with four categories: pure copper, CuCrZr, CuCrNb, and diamond-copper (diamond-copper was first shown at the Beijing Copper-Based Materials Conference in May and is now formally launched for 3D printing). Diamond-copper offers thermal conductivity more than twice that of pure copper and a coefficient of thermal expansion matched to chips, targeting thermal management applications such as liquid-cooling plates for AI computing, high-power electronic devices, and chip heat dissipation. Also exhibited were T70X high-temperature titanium alloy, VM7055/VAA450 high-strength aluminum alloys, and 0-25 μm MIM feedstock (stainless steel 316/304L/17-4, already in mass production). The completion of the four copper-based categories marks a shift by domestic powder manufacturers from single additive consumables toward the powder metallurgy and precision manufacturing supply chain; AI computing thermal management is currently the fastest-growing mainline for copper-based powders. For powder buyers: AI liquid-cooling plate and chip heat dissipation applications can directly request quotes for diamond-copper powder; MIM feedstock is already in mass production, offering consumer electronics and precision component customers an alternative to imports.