Belgian industrial additive manufacturing service provider AnyShape has been selected as a supplier of Scalmalloy components for the Airbus Eurodrone UAV program. Scalmalloy is a high-performance aluminum-magnesium-scandium alloy developed by Airbus subsidiary APWorks, offering strength comparable to titanium and density similar to aluminum, along with high specific strength, corrosion resistance, and microstructural stability above 250°C. AnyShape is one of only two Airbus-certified suppliers of Scalmalloy parts globally, utilizing selective laser melting and direct metal laser sintering technologies to produce flight hardware. The Eurodrone, one of Europe's largest defense projects, elevates the serial production application of Scalmalloy in lightweight aerospace structural components to new heights.