Poland-based 3D Lab has completed its NGAM project, using ultrasonic atomization technology to produce advanced aluminum alloy powder. In the final trial, the sieved fine powder achieved an average sphericity of 0.96, with a particle size distribution of D10=29.90 μm, D50=41.41 μm, and D90=55.37 μm, and preliminary printing validation was completed on 2onelab's PBF-LB equipment. This route explores the feasibility of producing aluminum alloy powder directly from scrap and pure elements, providing a technical reference for diversifying powder sources. 3D Lab previously debuted the ATO HUB multi-device powder production platform (an ultrasonic atomization production-line-level solution) with ARCWAY at Formnext. Value for buyers: the direct-from-scrap aluminum powder route has been validated as feasible through printing, and the 0.96 sphericity reaches a level suitable for PBF-LB — the cost-reduction path of producing powder from recycled aluminum scrap is worth tracking for aluminum powder buyers, and represents another technical option for diversifying low-cost aluminum powder supply in Europe.