Professor Li Yanle's team at the School of Mechanical Engineering, Shandong University, has recently made new progress in the field of equal-material–additive hybrid manufacturing, proposing an alternating hybrid manufacturing process that combines sheet incremental forming with laser directed energy deposition. The results were published in Int J Mach Tools Manuf (IF=24.1), a top journal in mechanical manufacturing. PhD student Ge Tingyu is the first author, Professor Li Yanle is the sole corresponding author, and Shandong University is the sole completing institution. Aiming at the needs of high-end equipment such as aerospace for lightweight, integrated, and high-performance manufacturing of complex metal components, the research developed a dual-robot collaborative processing equipment that organically integrates sheet incremental forming with laser directed energy deposition. Through multi-stage alternating processing, it achieves integrated and efficient manufacturing of complex curved thin-walled components and local functional features. By prefabricating local additive features and performing collaborative plastic forming, it achieves wall thickness compensation and local strengthening of thin-walled components in areas prone to thinning. The research also proposes macro- and micro-deformation and microstructure control methods for the equal-material–additive hybrid manufacturing process, establishes a segmented analytical model for incremental forming of hybrid sheets to reveal deformation mechanisms, clarifies microstructure evolution laws under different hybrid process routes, and suppresses additive thermal damage through dynamic recrystallization and residual stress reconstruction by controlling multi-stage plastic deformation. The team has achieved innovative progress on key scientific issues in equal-material–additive hybrid manufacturing, including active suppression of thermal deformation and interface strengthening and toughening of dissimilar materials. The results were published in International Journal of Plasticity, Virtual Phys Prototyp, J Manuf Process, J Mater Process Tech, and other journals. The team-led achievement 'Flexible Equal-Material–Additive Manufacturing Technology and Equipment Application for High-Performance Metal Components' won the Second Prize for Scientific and Technological Progress of the 2026 Machinery Industry Science and Technology Award. The project results have been applied by 12 units in aerospace, high-end equipment, and other fields, breaking through the technical bottleneck of low-cost rapid development of aerospace metal thin-walled components. Value for powder suppliers: equal-material–additive hybrid manufacturing expands new application scenarios for laser directed energy deposition (DED) powders for large components and thin-walled dissimilar structures. The demand for low-cost rapid development of aerospace titanium alloy thin-walled components will drive coordinated procurement of titanium alloy powders and equipment.