On November 25, HP announced the expansion of its Metal Jet binder jetting metal 3D printing material system, with new developments covering nickel-based superalloys, pure copper, and tungsten carbide, targeting aerospace, energy, and thermal management applications. The binder jetting (BJT) route is extending from being able to process stainless steel toward high-value engineering materials, and the importance of powder sintering characteristics and batch consistency in the BJT context is rising further, while the divergence from the powder qualification lists for the PBF route will become more pronounced. Value for powder suppliers: BJT powders require tighter particle size distribution and sintering window control, and powder grades that are first to pass HP material certification will lock in supply eligibility for this route.