A team led by Zhang Tianlong at the Hong Kong University of Science and Technology used LPBF in-situ alloying to build micrometer-scale molybdenum compositional waves within Ti-6Al-4V, forming three regions with different phase stabilities and opening a new paradigm in titanium alloy design. The design coordinates three deformation mechanisms — detwinning, stress-induced martensitic transformation, and dislocation slip. The Ti64-6Mo alloy achieves a work-hardening increment of about 557 MPa, more than twice the upper limit of conventional titanium alloys, with a tensile strength of 1,236 MPa and a uniform elongation of 11.5%. The results were published in Nature Communications. Technical value: this titanium alloy design approach substantially improves strength and plasticity simultaneously, providing a replicable paradigm for developing alloys dedicated to additive manufacturing.