17-4PH Stainless Steel Powder for Additive Manufacturing

✓ Verified

Stainless Steel · 17-4PH Stainless Steel · 53-150μm

Price Range / 价格区间

$21.00 - $24.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
17-4PH Stainless Steel
Particle Size
53-150μm
Process
PREP (Plasma Rotating Electrode Process)

Supplier / 供应商

N

NULL

China

Verified

Technical Specifications / 技术规格

Grade: 17-4PH Stainless Steel | PSD: 53-150μm | Process: PREP (Plasma Rotating Electrode Process)

Description / 产品描述

Premium 17-4PH Stainless Steel powder. ,,,