High Purity Spherical Aluminum Powder

Other · 高纯 40-180目 · +60 mesh: <8%, -200 mesh: ≤35%

Price Range / 价格区间

$0.00 - $0.00 / 元/公斤

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
高纯 40-180目
Particle Size
+60 mesh: <8%, -200 mesh: ≤35%
Process
N/A

Technical Specifications / 技术规格

Grade: 高纯 40-180目 | Particle Size: +60 mesh: <8%, -200 mesh: ≤35%