Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →
🔧

H13 Tool Steel Powder

Tool Steel · H13 · 15-53μm

Price Range / 价格区间

$0.00 - $0.00 / 元/公斤

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
H13
Particle Size
15-53μm
Process
参考标准值

Technical Specifications / 技术规格

Grade: H13 | Particle Size: 15-53μm | Process: 参考标准值 | Application: 参考标准值

Compare Similar Products

Product Particle Size Price (USD/kg) Supplier Certifications
H13 Tool Steel Powder Current 15-53μm $0 – $0 Avimetal Powder Technology —
18Ni300 Maraging Steel Powder for Tooling 15-53 μm $37 – $48 Weilaray Advanced Powder ✓ ISO 9001 Compare →

🔗 Related Tool Steel Products