Air Atomized Aluminum Powder
Other · FLPA250 · ≥250 μm
Price Range / 价格区间
$0.00
- $0.00 / per kg
MOQ: 10 kg
Lead Time: 7-14 days
● In Stock
Grade
FLPA250
Particle Size
≥250 μm
Process
干燥压缩空气雾化
Supplier / 供应商
A
Avimetal Powder Technology
Jiangsu, China
Technical Specifications / 技术规格
Grade: FLPA250 | PSD: >=250 μm | Process: | Applicat
Description / 产品描述
Air Atomized Aluminum Powder Suitable for .
🔗 Related Other Products
GNO High-purity Nickel Oxide
GNO-3 · <1 μm
$0/kg
🏭 Gansu Jinyi Micropowder Material Technology Co., Ltd.
Air Atomized Aluminum Powder
FLPA160A · ≥160 μm
$0/kg
🏭 Verified Chinese Supplier
Atomized Mg-RE Series Alloy Powder
Mg:Gd=90:10 · 100-300目 (50μm-150μm)
$0/kg
🏭 Verified Chinese Supplier
Pure Niobium Nb Spherical Powder
纯铌Nb · 15-53μm
$0/kg
🏭 Verified Chinese Supplier
Pure Hafnium Hf Spherical Powder
纯铪Hf · 15-53μm
$0/kg
🏭 Verified Chinese Supplier
Pure Zirconium Zr Spherical Powder
纯锆Zr · 15-53μm
$0/kg
🏭 Verified Chinese Supplier