Stainless Steel 316L Powder for Industrial AM
✓ Verified
Stainless Steel · 316L · 15-53 μm
Price Range / 价格区间
$29.50
- $37.50 / per kg
MOQ: 25 kg
Lead Time: 3-5 days
● In Stock
Grade
316L
Particle Size
15-53 μm
Process
VIGA
Technical Specifications / 技术规格
Chemical: Fe Bal, Cr 16.0-18.0%, Ni 10.0-14.0%, Mo 2.0-3.0%, C <=0.03% | PSD: 15-53 μm | App Density: >=3.9 g/cm³ | Flow: <=22 s/50g | O2: <=200 ppm | UTS: 500-670 MPa
Description / 产品描述
High-quality 316L austenitic stainless steel powder. Most widely used material in metal AM. Excellent corrosion resistance, good mechanical properties, competitive pricing.
Compare Similar Products
| Product | Particle Size | Price (USD/kg) | Supplier | Certifications | |
|---|---|---|---|---|---|
| Stainless Steel 316L Powder for Industrial AM Current | 15-53 μm | $30 – $38 | Weilaray Advanced Powder ✓ | ISO 9001 | |
| 316L Stainless Steel Powder for Additive Manufacturing | 15-53μm | $8 – $9 | Inner Mongolia Sunruns New Material Co., Ltd. ✓ | — | Compare → |
| 7075 Aluminum Alloy Powder for Additive Manufacturing | 0-25um | $18 – $26 | Hunan AoKe New Material Technology Co., Ltd. ✓ | — | Compare → |
| 20Cr13 Stainless Steel Powder for Additive Manufacturing | 53-150μm | $21 – $24 | NULL ✓ | — | Compare → |
| H13 Hot Work Tool Steel Powder for Additive Manufacturing | 53-150μm | $21 – $24 | NULL ✓ | — | Compare → |
| GCr15 Bearing Steel Powder for Additive Manufacturing | 53-150μm | $21 – $24 | NULL ✓ | — | Compare → |
📊 Price Trend — Stainless Steel
Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.
🔗 Related Stainless Steel Products
316L Stainless Steel Powder for Additive Manufacturing
316L Stainless Steel · 15-53μm
$8–$9/kg
✓ Verified
🏭 Inner Mongolia Sunruns New Material Co., Ltd.
7075 Aluminum Alloy Powder for Additive Manufacturing
7075 Aluminum Alloy · 0-25um
$18–$26/kg
✓ Verified
🏭 Hunan AoKe New Material Technology Co., Ltd.
42CrMo Alloy Steel Powder for Additive Manufacturing
42CrMo Alloy Steel · 53-150μm
$21–$24/kg
✓ Verified
🏭 NULL
H13 Hot Work Tool Steel Powder for Additive Manufacturing
H13 Hot Work Tool Steel · 53-150μm
$21–$24/kg
✓ Verified
🏭 NULL
17-4PH Stainless Steel Powder for Additive Manufacturing
17-4PH Stainless Steel · 53-150μm
$21–$24/kg
✓ Verified
🏭 NULL
4Cr13 Martensitic Stainless Steel Powder for Additive Manufacturing
4Cr13 Martensitic Stainless Steel · 53-150μm
$21–$24/kg
✓ Verified
🏭 NULL