At the 2026 Sci-Tech Innovation and Industrial High-Quality Development Conference held in Changzhou on August 29, Vilary was honored with the "New Quality Enterprise Golden Bull Award" by China Securities Journal (as reported by Xukuang Media on September 7). The company's EIGA/VIGA powder production equipment has achieved 100% self-sufficiency and independent control. Notably, Vilary developed China's first 600-kilogram-class intelligent powder production system, and its T70X high-temperature titanium alloy powder, capable of stable service at 700°C, fills a domestic gap for large-format, high-temperature-resistant titanium alloys. With over 200 authorized patents and leadership in more than 20 national standards, the company has reversed its high-end metal powder supply from 90% imported to 90% domestically developed. Titanium alloy powder prices have plummeted from tens of thousands of yuan per kilogram to just hundreds. Once its Phase III and IV facilities are completed, annual production capacity is set to exceed 10,000 tons.