Nantong Jingcheng Intelligence Technology Co., Ltd. has initiated the environmental impact assessment for a project with an annual output of 100 tons of metal 3D-printed parts and 200 tons of titanium alloy MIM (Metal Injection Molding) parts. Located in Nantong Economic and Technological Development Zone, Jiangsu Province, the project plans to establish an 'Industrial Metal 3D Printing Processing Center' and a titanium alloy MIM production line, adopting dual technical routes of metal 3D printing and MIM. Metal 3D printing targets high-value-added applications such as aerospace structural components and industrial parts, while MIM parts focus on mass production of small precision components for consumer electronics and medical devices.