AMAZEMET will showcase a standalone laser ultrasonic atomization powder production system at Formnext 2026, capable of producing metal powders such as Ti-6Al-4V. AMAZEMET originated as a spin-off from Warsaw University of Technology in Poland and focuses on metal additive manufacturing and powder production equipment. Laser ultrasonic atomization is a further powder production technology route following gas atomization and plasma atomization: a high-energy laser melts the metal and ultrasonic vibration breaks the melt into fine droplets, which solidify into spherical powder. Compared with conventional gas atomization, it requires no high-pressure gas flow system, has a smaller equipment footprint and lower safety requirements, offers flexible material changeover, and suits multi-grade small-batch production. It can support universities and companies in producing their own experimental powders and shorten material R&D iteration cycles. Sphericity and particle size distribution can be jointly controlled through laser power and ultrasonic parameters, and the standalone system format indicates that the process is moving from the laboratory toward production lines. The emergence of a new powder production process route may, in the medium to long term, change the supply landscape for high-end spherical powders, and domestic powder equipment manufacturers can track and benchmark its principles and parameters.