Farsoon Europe has partnered with Korevo to develop metal additive manufacturing process parameters for industrial molds, based on the FS273M-2 machine and targeting conformal cooling mold applications across injection molding and die casting scenarios. Conventional machined cooling channels can only be drilled as straight holes and cannot follow complex cavity shapes, and uneven cooling leads to longer injection molding cycles and warpage defects. Metal additive manufacturing can form conformal channels that follow the cavity contour, significantly improving cooling uniformity and production efficiency. The associated powders are mostly mold steel grades such as H13 hot work die steel and 18Ni300 maraging steel, and conformal cooling can also extend mold life. Korevo is a service provider in the mold sector, and the joint development will distill Farsoon's equipment capabilities into a reusable industry parameter library, lowering the barrier for mold makers to adopt metal additive manufacturing. Domestic equipment leaders are going global with an equipment-plus-process-parameters model that binds downstream applications, expanding opportunities for domestically produced powders to enter the European mold supply chain alongside equipment installations.