Srui New Materials (688102) has been granted an invention patent for "A Manufacturing Method for the Inner and Outer Walls of a Liquid Rocket Engine Thrust Chamber." The patent application number is CN202511519460.X, and the grant date is November 13, 2026. Process route: first, a multi-pass spinning process is used to prepare a copper alloy inner-wall workpiece with cooling channels; the cooling channels are then filled and protected with a high-temperature peelable filler material composed of a heat-resistant filler, a binder, and a carrier additive; next, an outer-wall layer is formed on the surface of the filled body by cold spraying stainless steel or superalloy powder with a particle size of 15 to 45 micrometers at a gas temperature of 600 to 900 degrees Celsius and a pressure of 3 to 5 MPa. The filler is then removed, and densification is achieved by hot isostatic pressing at 920 to 980 degrees Celsius and 150 MPa for 2 to 6 hours; finally, electrolytic polishing of 10 to 30 micrometers yields the thrust chamber inner- and outer-wall assembly. Through control of the combined process parameters of spinning, cold spraying, and hot isostatic pressing, weld-free integrated manufacturing is achieved, solving problems such as weld failure in conventional processes, low material utilization, and defects in additive manufacturing. Since the start of this year, the company has added 32 granted patents, a year-on-year increase of 77.78%; in the first half of 2026, R&D investment was 57.1346 million yuan, up 34.74% year on year, indicating its continued technical investment in the manufacturing of liquid rocket engine thrust chambers.