A joint research team comprising Zhong Han Wong, Jonathan Aristya, Mingyong Jia, Jinxi Guo, Yang Yang and Xipeng Tan has published a study titled Direct observation of surface chemistry evolution for Ti-6Al-4V powders in calciothermic reduction recycling process in npj Materials Degradation. The paper was officially released on 13 November 2026 under DOI 10.1038/s41529-026-00903-8 and is available as open access. The study focuses on the surface chemistry evolution of Ti-6Al-4V titanium alloy powders during the calciothermic reduction recycling process, using direct observation methods to track changes in the chemical state of powder particle surfaces throughout recycling treatment. The work characterizes the phase and chemical behavior of powder surfaces under this calciothermic reduction recycling route. The paper was published online as an accelerated article preview and falls within the fields of engineering and materials science. Ti-6Al-4V is one of the most widely used titanium alloy grades in metal additive manufacturing, and the surface chemistry of its powder directly affects performance in subsequent printing cycles. Using recycled powder as its subject, the study directly observes the evolution pathway of powder surface chemistry during calciothermic reduction, providing a reference methodology for characterizing the surface state of titanium alloy powders in closed-loop recycling.